COPPER BONDED SOLID EARTH ROD

SALIENT FEATURES

  • Permanent Molecular Bonding of 99.9% Pure Electrolytic Copper
  • Low Carbon Steel Core for Greater Tensile Strength
  • Copper Bonding (100 microns+ minimum | 254 microns+)
  • Minimum Copper Coating of 254 Microns (10 Mil) on Rods Listed to UL467
  •  Cold-Rolled Threads with Continuous, Unbroken Grain flows preserve Copper Coating and are Stronger than Cut Threads (for Threaded Rods)
  • Maintenance Free and Corrosion Resistant
  • Low Resistance Guaranteed
  • High Fault Current Capacity
  • Cost-Effective & Long Service Life
  • Deep Driving Capability
  • Copper Bonding will not Crack when Bent or Tear when Driving
  • LATH Brand Name, Model Number, Diameter, Length are Laser Marked
  • Available along with Test cum Guarantee Certificate and Earth Pit Display Label

WHY LATH?

  • 10 YEARS REPLACEMENT AND PERFORMANCE GUARANTEE".
  • In-house Cold Drawn Bright Round processing facility for Stringent Quality Control.
  • Raw Materials sourced from Integrated Steel Producers i.e. JSW & Vizag Steel Plant (RINL) only.
  • No Minus Tolerance on Diameter and Length of the Rod i.e, 17.2mm means 17.2mm not 16mm.
  • Clamp is fully welded using only ADOR or ESAB MIG Welding & its Consumables.
  • Having Minimum 100 Microns + Copper Bonding prevents Rusting and Corrosion (No False Claim of Higher Copper Coating, Coating available as Committed).
  • All our Products are Laser Marked as a Testimonial of Performance & Guarantee.

PRODUCT SPECIFICATION

TESTS PASSED

CPRI, BANGALORE

  • Tested Short-time withstand current and Peak withstand current
    (15kA RMS for 1.03 & 37.5kA Peak)

UL, BANGALORE (U L467)

  • Thickness of Protective Coating test (254 microns+)
  • Adherence of Coating Test (No Peel Off)
  • Bending Test (No Cracks)

NABL ACCREDITED LABORATORY

  • Bend Test (No Cracks or Deformation)
  • Adhesion Test (Knife Test) No Peel Off
  • Cooper Plating Thickness (254 microns+)

Meets the requirement of IS 3043, IEC 62561-2 and UL467